Mechanical Properties
( Sand Cast ) |
|
Tensile |
60,000 psi |
|
Yield |
24,000 psi |
|
Elongation |
22% |
|
Machinability Rating |
80% |
| |
Eco Brass
Sand Casting Version Specification |
Nominal
Specification |
|
Copper |
74 – 78 |
76.0 |
|
Tin |
.30 |
|
|
Lead |
.10 |
|
|
Zinc |
Remainder |
20.9 |
|
Silicon |
2.7 – 3.4 |
3.0 |
|
Phosphorus |
0.05 - .20 |
.12 |
|
 |